“Photocatalytic acetaldehyde oxidation in air using spacious TiO2 films prepared by atomic layer deposition on supported carbonaceous sacrificial templates”. Verbruggen SW, Deng S, Kurttepeli M, Cott DJ, Vereecken PM, Bals S, Martens JA, Detavernier C, Lenaerts S, Applied catalysis : B : environmental 160, 204 (2014). http://doi.org/10.1016/j.apcatb.2014.05.029
Abstract: Supported carbon nanosheets and carbon nanotubes served as sacrificial templates for preparing spacious TiO2 photocatalytic thin films. Amorphous TiO2 was deposited conformally on the carbonaceous template material by atomic layer deposition (ALD). Upon calcination at 550 °C, the carbon template was oxidatively removed and the as-deposited continuous amorphous TiO2 layers transformed into interlinked anatase nanoparticles with an overall morphology commensurate to the original template structure. The effect of type of template, number of ALD cycles and gas residence time of pollutant on the photocatalytic activity, as well as the stability of the photocatalytic performance of these thin films was investigated. The TiO2 films exhibited excellent photocatalytic activity toward photocatalytic degradation of acetaldehyde in air as a model reaction for photocatalytic indoor air pollution abatement. Optimized films outperformed a reference film of commercial PC500.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT); Sustainable Energy, Air and Water Technology (DuEL)
Impact Factor: 9.446
Times cited: 37
DOI: 10.1016/j.apcatb.2014.05.029
|
|
|
“Silver-polymer core-shell nanoparticles for ultrastable plasmon-enhanced photocatalysis”. Asapu R, Claes N, Bals S, Denys S, Detavernier C, Lenaerts S, Verbruggen SW, Applied catalysis : B : environmental 200, 31 (2017). http://doi.org/10.1016/j.apcatb.2016.06.062
Abstract: Affordable silver-polymer core-shell nanoparticles are prepared using the layer-by-layer (LbL) technique. The metallic silver core is encapsulated with an ultra-thin protective shell that prevents oxidation and clustering without compromising the plasmonic properties. The core-shell nanoparticles retain their plasmonic near field enhancement effect, as studied from finite element numerical simulations. Control over the shell thickness up to the sub-nanometer level is there for key. The particles are used to prepare a plasmonic Ag-TiO2 photocatalyst of which the gas phase photocatalytic activity is monitored over a period of four months. The described system outperforms pristine TiO2 and retains its plasmonic enhancement in contrast to TiO2 modified with bare silver nanoparticles. With this an important step is made toward the development of long-term stable plasmonic (photocatalytic) applications.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT); Sustainable Energy, Air and Water Technology (DuEL)
Impact Factor: 9.446
Times cited: 45
DOI: 10.1016/j.apcatb.2016.06.062
|
|
|
“Plasmonic gold-embedded TiO2 thin films as photocatalytic self-cleaning coatings”. Peeters H, Keulemans M, Nuyts G, Vanmeert F, Li C, Minjauw M, Detavernier C, Bals S, Lenaerts S, Verbruggen SW, Applied Catalysis B-Environmental 267, 118654 (2020). http://doi.org/10.1016/j.apcatb.2020.118654
Abstract: Transparent photocatalytic TiO2 thin films hold great potential in the development of self-cleaning glass sur-
faces, but suffer from a poor visible light response that hinders the application under actual sunlight. To alleviate this problem, the photocatalytic film can be modified with plasmonic nanoparticles that interact very effectively with visible light. Since the plasmonic effect is strongly concentrated in the near surroundings of the nano- particle surface, an approach is presented to embed the plasmonic nanostructures in the TiO2 matrix itself, rather than deposit them loosely on the surface. This way the interaction interface is maximised and the plasmonic effect can be fully exploited. In this study, pre-fabricated gold nanoparticles are made compatible with the organic medium of a TiO2 sol-gel coating suspension, resulting in a one-pot coating suspension. After spin coating, homogeneous, smooth, highly transparent and photoactive gold-embedded anatase thin films are ob- tained.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT); AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation); Sustainable Energy, Air and Water Technology (DuEL)
Impact Factor: 22.1
Times cited: 57
DOI: 10.1016/j.apcatb.2020.118654
|
|
|
“Oxidation barrier of Cu and Fe powder by Atomic Layer Deposition”. Cremers V, Rampelberg G, Barhoum A, Walters P, Claes N, Oliveira TM de, Assche GV, Bals S, Dendooven J, Detavernier C, Surface and coatings technology 349, 1032 (2018). http://doi.org/10.1016/j.surfcoat.2018.06.048
Abstract: Atomic layer deposition (ALD) is a vapor based technique which allows to deposit uniform, conformal films with a thickness control at the atomic scale. In this research, Al 2 O 3 coatings were deposited on micrometer-sized Fe and Cu powder (particles) using the thermal trimethylaluminum (TMA)/ water (H 2 O) process in a rotary pump-type ALD reactor. Rotation of the powder during deposition was required to obtain a pinhole-free ALD coating. The protective nature of the coating was evaluated by quantifying its effectiveness in protecting the metal particles during oxidative annealing treatments. The Al 2 O 3 coated powders were annealed in ambient air while in-situ thermogravimetric analysis (TGA) and in-situ x-ray diffraction (XRD) data were acquired. The thermal stability of a series of Cu and Fe powder with different Al 2 O 3 thicknesses were determined with TGA. In both samples a clear shift in oxidation temperature is visible. For Cu and Fe powder coated with 25 nm Al 2 O 3 , we observed an increase of the oxidation temperature with 300-400°C. For the Cu powder a thin film of only 8 nm is required to obtain an initial increase in oxidation temperature of 200°C. In contrast, for Fe powder a thicker coating of 25 nm is required. In both cases, the oxidation temperature increases with increasing thickness of the Al 2 O 3 coating. These results illustrate that the Al 2 O 3 thin film, deposited by the thermal ALD process (TMA/H 2 O) can be an efficient and pinhole-free barrier layer for micrometer-sized powder particles, provided that the powder is properly agitated during the process to ensure sufficient vapour-solid interaction.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 2.589
Times cited: 10
DOI: 10.1016/j.surfcoat.2018.06.048
|
|