“Induced giant piezoelectricity in centrosymmetric oxides”. Park D-s, Hadad M, Riemer LM, Ignatans R, Spirito D, Esposito V, Tileli V, Gauquelin N, Chezganov D, Jannis D, Verbeeck J, Gorfman S, Pryds N, Muralt P, Damjanovic D, Science 375, 653 (2022). http://doi.org/10.1126/science.abm7497
Abstract: Giant piezoelectricity can be induced in centrosymmetric oxides by controlling the long-range motion of oxygen vacancies.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 56.9
Times cited: 51
DOI: 10.1126/science.abm7497
|
|
|
“Germanium vacancy centre formation in CVD nanocrystalline diamond using a solid dopant source”. Mary Joy R, Pobedinskas P, Bourgeois E, Chakraborty T, Görlitz J, Herrmann D, Noël C, Heupel J, Jannis D, Gauquelin N, D'Haen J, Verbeeck J, Popov C, Houssiau L, Becher C, Nesládek M, Haenen K, Science talks 5, 100157 (2023). http://doi.org/10.1016/j.sctalk.2023.100157
Keywords: A3 Journal article; Electron microscopy for materials research (EMAT)
DOI: 10.1016/j.sctalk.2023.100157
|
|
|
“Controlled growth of hexagonal gold nanostructures during thermally induced self-assembling on Ge(001) surface”. Jany BR, Gauquelin N, Willhammar T, Nikiel M, van den Bos KHW, Janas A, Szajna K, Verbeeck J, Van Aert S, Van Tendeloo G, Krok F, Scientific reports 7, 42420 (2017). http://doi.org/10.1038/srep42420
Abstract: Nano-sized gold has become an important material in various fields of science and technology, where control over the size and crystallography is desired to tailor the functionality. Gold crystallizes in the face-centered cubic (fcc) phase, and its hexagonal closed packed (hcp) structure is a very unusual and rare phase. Stable Au hcp phase has been reported to form in nanoparticles at the tips of some Ge nanowires. It has also recently been synthesized in the form of thin graphene-supported sheets which are unstable under electron beam irradiation. Here, we show that stable hcp Au 3D nanostructures with well-defined crystallographic orientation and size can be systematically created in a process of thermally induced self-assembly of thin Au layer on Ge(001) monocrystal. The Au hcp crystallite is present in each Au nanostructure and has been characterized by different electron microscopy techniques. We report that a careful heat treatment above the eutectic melting temperature and a controlled cooling is required to form the hcp phase of Au on a Ge single crystal. This new method gives scientific prospects to obtain stable Au hcp phase for future applications in a rather simple manner as well as redefine the phase diagram of Gold with Germanium.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 4.259
Times cited: 25
DOI: 10.1038/srep42420
|
|
|
“Interfacial dielectric layer as an origin of polarization fatigue in ferroelectric capacitors”. Do MT, Gauquelin N, Nguyen MD, Wang J, Verbeeck J, Blom F, Koster G, Houwman EP, Rijnders G, Scientific Reports 10, 7310 (2020). http://doi.org/10.1038/s41598-020-64451-0
Abstract: Origins of polarization fatigue in ferroelectric capacitors under electric field cycling still remain unclear. Here, we experimentally identify origins of polarization fatigue in ferroelectric PbZr0.52Ti0.48O3 (PZT) thin-film capacitors by investigating their fatigue behaviours and interface structures. The PZT layers are epitaxially grown on SrRuO3-buffered SrTiO3 substrates by a pulsed laser deposition (PLD), and the capacitor top-electrodes are various, including SrRuO3 (SRO) made by in-situ PLD, Pt by in-situ PLD (Pt-inPLD) and ex-situ sputtering (Pt-sputtered). We found that fatigue behaviour of the capacitor is directly related to the top-electrode/PZT interface structure. The Pt-sputtered/PZT/SRO capacitor has a thin defective layer at the top interface and shows early fatigue while the Pt-inPLD/PZT/SRO and SRO/PZT/SRO capacitor have clean top-interfaces and show much more fatigue resistance. The defective dielectric layer at the Pt-sputtered/PZT interface mainly contains carbon contaminants, which form during the capacitor ex-situ fabrication. Removal of this dielectric layer significantly delays the fatigue onset. Our results clearly indicate that dielectric layer at ferroelectric capacitor interfaces is the main origin of polarization fatigue, as previously proposed in the charge injection model.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 4.6
Times cited: 18
DOI: 10.1038/s41598-020-64451-0
|
|
|
“Gate-tuned anomalous Hall effect driven by Rashba splitting in intermixed LaAlO3/GdTiO3/SrTiO3”. Lebedev N, Stehno M, Rana A, Reith P, Gauquelin N, Verbeeck J, Hilgenkamp H, Brinkman A, Aarts J, Scientific Reports 11, 10726 (2021). http://doi.org/10.1038/s41598-021-89767-3
Abstract: The Anomalous Hall Effect (AHE) is an important quantity in determining the properties and understanding the behaviour of the two-dimensional electron system forming at the interface of SrTiO<sub>3</sub>-based oxide heterostructures. The occurrence of AHE is often interpreted as a signature of ferromagnetism, but it is becoming more and more clear that also paramagnets may contribute to AHE. We studied the influence of magnetic ions by measuring intermixed LaAlO<sub>3</sub>/GdTiO<sub>3</sub>/SrTiO<sub>3</sub>at temperatures below 10 K. We find that, as function of gate voltage, the system undergoes a Lifshitz transition while at the same time an onset of AHE is observed. However, we do not observe clear signs of ferromagnetism. We argue the AHE to be due to the change in Rashba spin-orbit coupling at the Lifshitz transition and conclude that also paramagnetic moments which are easily polarizable at low temperatures and high magnetic fields lead to the presence of AHE, which needs to be taken into account when extracting carrier densities and mobilities.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 4.259
Times cited: 5
DOI: 10.1038/s41598-021-89767-3
|
|
|
“Tailoring mechanical properties and shear band propagation in ZrCu metallic glass nanolaminates through chemical heterogeneities and interface density”. Brognara A, Kashiwar A, Jung C, Zhang X, Ahmadian A, Gauquelin N, Verbeeck J, Djemia P, Faurie D, Dehm G, Idrissi H, Best JP, Ghidelli M, Small Structures , 2400011 (2024). http://doi.org/10.1002/SSTR.202400011
Abstract: The design of high‐performance structural thin films consistently seeks to achieve a delicate equilibrium by balancing outstanding mechanical properties like yield strength, ductility, and substrate adhesion, which are often mutually exclusive. Metallic glasses (MGs) with their amorphous structure have superior strength, but usually poor ductility with catastrophic failure induced by shear bands (SBs) formation. Herein, we introduce an innovative approach by synthesizing MGs characterized by large and tunable mechanical properties, pioneering a nanoengineering design based on the control of nanoscale chemical/structural heterogeneities. This is realized through a simplified model Zr 24 Cu 76 /Zr 61 Cu 39 , fully amorphous nanocomposite with controlled nanoscale periodicity ( Λ , from 400 down to 5 nm), local chemistry, and glass–glass interfaces, while focusing in‐depth on the SB nucleation/propagation processes. The nanolaminates enable a fine control of the mechanical properties, and an onset of crack formation/percolation (>1.9 and 3.3%, respectively) far above the monolithic counterparts. Moreover, we show that SB propagation induces large chemical intermixing, enabling a brittle‐to‐ductile transition when Λ ≤ 50 nm, reaching remarkably large plastic deformation of 16% in compression and yield strength ≈2 GPa. Overall, the nanoengineered control of local heterogeneities leads to ultimate and tunable mechanical properties opening up a new approach for strong and ductile materials.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
DOI: 10.1002/SSTR.202400011
|
|
|
“Deeper insights into the photoluminescence properties and (photo)chemical reactivity of cadmium red (CdS1-xSex) paints in renowned twentieth century paintings by state-of-the-art investigations at multiple length scales”. Monico L, Rosi F, Vivani R, Cartechini L, Janssens K, Gauquelin N, Chezganov D, Verbeeck J, Cotte M, D'Acapito F, Barni L, Grazia C, Buemi LP, Andral J-L, Miliani C, Romani A, The European Physical Journal Plus 137, 311 (2022). http://doi.org/10.1140/EPJP/S13360-022-02447-7
Abstract: Cadmium red is the name used for denoting a class of twentieth century artists' pigments described by the general formula CdS1-xSex. For their vibrant hues and excellent covering power, a number of renowned modern and contemporary painters, including Jackson Pollock, often used cadmium reds. As direct band gap semiconductors, CdS1-xSex compounds undergo direct radiative recombination (with emissions from the green to orange region) and radiative deactivation from intragap trapping states due to crystal defects, which give rise to two peculiar red-NIR emissions, known as deep level emissions (DLEs). The positions of the DLEs mainly depend on the Se content of CdS1-xSex; thus, photoluminescence and diffuse reflectance vis-NIR spectroscopy have been profitably used for the non-invasive identification of different cadmium red varieties in artworks over the last decade. Systematic knowledge is however currently lacking on what are the parameters related to intrinsic crystal defects of CdS1-xSex and environmental factors influencing the spectral properties of DLEs as well as on the overall (photo)chemical reactivity of cadmium reds in paint matrixes. Here, we present the application of a novel multi-length scale and multi-method approach to deepen insights into the photoluminescence properties and (photo)chemical reactivity of cadmium reds in oil paintings by combining both well established and new non-invasive/non-destructive analytical techniques, including macro-scale vis-NIR and vibrational spectroscopies and micro-/nano-scale advanced electron microscopy mapping and X-ray methods employing synchrotron radiation and conventional sources. Macro-scale vis-NIR spectroscopy data obtained from the in situ non-invasive analysis of nine masterpieces by Gerardo Dottori, Jackson Pollock and Nicolas de Stael allowed classifying the CdS1-xSex-paints in three groups, according to the relative intensity of the two DLE bands. These outcomes, combined with results from micro-/nano-scale electron microscopy mapping and X-ray analysis of a set of CdS1-xSex powders and artificially aged paint mock-ups, indicated that the relative intensity of DLEs is not affected by the morphology, microstructure and local atomic environment of the pigment particles but it is influenced by the presence of moisture. Furthermore, the extensive study of artificially aged oil paint mock-ups permitted us to provide first evidence of the tendency of cadmium reds toward photo-degradation and to establish that the conversion of CdS1-xSex to CdSO4 and/or oxalates is triggered by the oil binding medium and moisture level and depends on the Se content. Based on these findings, we could interpret the localized presence of CdSO4 and cadmium oxalate as alteration products of the original cadmium red paints in two paintings by Pollock.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT); Antwerp X-ray Imaging and Spectroscopy (AXIS)
Impact Factor: 3.4
Times cited: 3
DOI: 10.1140/EPJP/S13360-022-02447-7
|
|
|
“Chemical structure of nitrogen-doped graphene with single platinum atoms and atomic clusters as a platform for the PEMFC electrode”. Stambula S, Gauquelin N, Bugnet M, Gorantla S, Turner S, Sun S, Liu J, Zhang G, Sun X, Botton GA, The journal of physical chemistry: C : nanomaterials and interfaces 118, 3890 (2014). http://doi.org/10.1021/jp408979h
Abstract: A platform for producing stabilized Pt atoms and clusters through the combination of an N-doped graphene support and atomic layer deposition (ALD) for the Pt catalysts was investigated using transmission electron microscopy (TEM) and scanning transmission electron microscopy (STEM). It was determined, using imaging and spectroscopy techniques, that a wide range of N-dopant types entered the graphene lattice through covalent bonds without largely damaging its structure. Additionally and most notably, Pt atoms and atomic clusters formed in the absence of nanoparticles. This work provides a new strategy for experimentally producing stable atomic and subnanometer cluster catalysts, which can greatly assist the proton exchange membrane fuel cell (PEMFC) development by producing the ultimate surface area to volume ratio catalyst.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 4.536
Times cited: 57
DOI: 10.1021/jp408979h
|
|
|
“Atomic resolution mapping of phonon excitations in STEM-EELS experiments”. Egoavil R, Gauquelin N, Martinez GT, Van Aert S, Van Tendeloo G, Verbeeck J, Ultramicroscopy 147, 1 (2014). http://doi.org/10.1016/j.ultramic.2014.04.011
Abstract: Atomically resolved electron energy-loss spectroscopy experiments are commonplace in modern aberration-corrected transmission electron microscopes. Energy resolution has also been increasing steadily with the continuous improvement of electron monochromators. Electronic excitations however are known to be delocalized due to the long range interaction of the charged accelerated electrons with the electrons in a sample. This has made several scientists question the value of combined high spatial and energy resolution for mapping interband transitions and possibly phonon excitation in crystals. In this paper we demonstrate experimentally that atomic resolution information is indeed available at very low energy losses around 100 meV expressed as a modulation of the broadening of the zero loss peak. Careful data analysis allows us to get a glimpse of what are likely phonon excitations with both an energy loss and gain part. These experiments confirm recent theoretical predictions on the strong localization of phonon excitations as opposed to electronic excitations and show that a combination of atomic resolution and recent developments in increased energy resolution will offer great benefit for mapping phonon modes in real space.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 2.843
Times cited: 22
DOI: 10.1016/j.ultramic.2014.04.011
|
|
|
“Determining oxygen relaxations at an interface: A comparative study between transmission electron microscopy techniques”. Gauquelin N, van den Bos KHW, Béché, A, Krause FF, Lobato I, Lazar S, Rosenauer A, Van Aert S, Verbeeck J, Ultramicroscopy 181, 178 (2017). http://doi.org/10.1016/j.ultramic.2017.06.002
Abstract: Nowadays, aberration corrected transmission electron microscopy (TEM) is a popular method to characterise nanomaterials at the atomic scale. Here, atomically resolved images of nanomaterials are acquired, where the contrast depends on the illumination, imaging and detector conditions of the microscope. Visualization of light elements is possible when using low angle annular dark field (LAADF) STEM, annular bright field (ABF) STEM, integrated differential phase contrast (iDPC) STEM, negative spherical aberration imaging (NCSI) and imaging STEM (ISTEM). In this work, images of a NdGaO3-La0.67Sr0.33MnO3 (NGO-LSMO) interface are quantitatively evaluated by using statistical parameter estimation theory. For imaging light elements, all techniques are providing reliable results, while the techniques based on interference contrast, NCSI and ISTEM, are less robust in terms of accuracy for extracting heavy column locations. In term of precision, sample drift and scan distortions mainly limits the STEM based techniques as compared to NCSI. Post processing techniques can, however, partially compensate for this. In order to provide an outlook to the future, simulated images of NGO, in which the unavoidable presence of Poisson noise is taken into account, are used to determine the ultimate precision. In this future counting noise limited scenario, NCSI and ISTEM imaging will provide more precise values as compared to the other techniques, which can be related to the mechanisms behind the image recording.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 2.843
Times cited: 34
DOI: 10.1016/j.ultramic.2017.06.002
|
|
|
“Atom column detection from simultaneously acquired ABF and ADF STEM images”. Fatermans J, den Dekker Aj, Müller-Caspary K, Gauquelin N, Verbeeck J, Van Aert S, Ultramicroscopy 219, 113046 (2020). http://doi.org/10.1016/j.ultramic.2020.113046
Abstract: In electron microscopy, the maximum a posteriori (MAP) probability rule has been introduced as a tool to determine the most probable atomic structure from high-resolution annular dark-field (ADF) scanning transmission electron microscopy (STEM) images exhibiting low contrast-to-noise ratio (CNR). Besides ADF imaging, STEM can also be applied in the annular bright-field (ABF) regime. The ABF STEM mode allows to directly visualize light-element atomic columns in the presence of heavy columns. Typically, light-element nanomaterials are sensitive to the electron beam, limiting the incoming electron dose in order to avoid beam damage and leading to images exhibiting low CNR. Therefore, it is of interest to apply the MAP probability rule not only to ADF STEM images, but to ABF STEM images as well. In this work, the methodology of the MAP rule, which combines statistical parameter estimation theory and model-order selection, is extended to be applied to simultaneously acquired ABF and ADF STEM images. For this, an extension of the commonly used parametric models in STEM is proposed. Hereby, the effect of specimen tilt has been taken into account, since small tilts from the crystal zone axis affect, especially, ABF STEM intensities. Using simulations as well as experimental data, it is shown that the proposed methodology can be successfully used to detect light elements in the presence of heavy elements.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT); Vision lab
Impact Factor: 2.2
Times cited: 9
DOI: 10.1016/j.ultramic.2020.113046
|
|