“High reflective mirrors for in-vessel applications in ITER”. Razdobarin AG, Mukhin EE, Semenov VV, YuTolstyakov S, Kochergin MM, Kurskiev GS, Podushnikova KA, Kirilenko DA, Sitnikova AA, Gorodetsky АЕ, Bukhovets VL, Zalavutdinov RK, Zakharov АP, Arkhipov II, Voitsenya VS, Bondarenko VN, Konovalov VG, Ryzhkov IV;, Nuclear instruments and methods in physics research : A: accelerators, spectrometers, detectors and associated equipment 623, 809 (2010). http://doi.org/10.1016/j.nima.2010.04.047
Abstract: The structure and surface morphology of aluminum and silver mirrors covered with protective dielectric oxide layer were studied by means of TEM and SEM. The presence of needle-like pores throughout the thickness of the ZrO(2) film and bubble-like pores in Al(2)O(3) was observed. The test for resistivity to deuterium ion bombardment shows that the exposition to a fluence of similar to 2 x 10(20) ions/cm(2) with the ion energy of 40-50 eV results in appearance of blisters on the surface of mirrors covered wit h Al(2)O(3). For the mirrors protected with ZrO(2) no noticeable changes in surface morphology and reflectivity were found even after order of magnitude higher ion fluence. The effect of different porous structures on blistering phenomena is discussed. (C) 2010 Elsevier B.V. All rights reserved.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 1.362
Times cited: 4
DOI: 10.1016/j.nima.2010.04.047
|
“Diagnostic mirrors with transparent protection layer for ITER”. Razdobarin AG, Mukhin EE, Semenov VV, Tolstyakov SY, Kochergin MM, Kurskiev GS, Podushnikova KA, Kirilenko DA, Sitnikova AA, Konovalov VG, Solodovchenko SI, Nekhaieva OM, Skorik OA, Bondarenko VN, Voitsenya VS;, Fusion engineering and design 86, 1341 (2011). http://doi.org/10.1016/j.fusengdes.2011.02.052
Abstract: Fast degradation of in-vessel optics is one of the most serious problems for all optical diagnostics in ITER. To provide the resistance to mechanical and thermal stresses along with a high stability of optical characteristics under deposition-dominated conditions we suggest using high-reflective metallic (Ag or Al) film mirrors coated on silicon substrate and protected with thin oxide film in the divertor Thomson Scattering (TS) diagnostics. The mirrors coated with Al2O3 and ZrO2 films were tested under irradiation by deuterium ions. The experimental results on the oxide films sputtering are discussed in the context of their applicability for the first mirror protection in ITER.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 1.319
Times cited: 6
DOI: 10.1016/j.fusengdes.2011.02.052
|