Abstract: The fine balance between dipole-field energy and anion drift force defines the switching mechanism during polarization reversal: for the first time we show that only Pbcm mechanism obeys the ferroelectric switching physics, whereas P4(2)/nmc (or any other) mechanism does not. However, with lower energy barrier, it represents an important antiferroelectric mechanism. Constraints relaxation can lead to 90 degrees polarization rotation (domain deactivation). Intrinsically, the Si/VO-doping can switch faster than undoped HfO2 or HfZrOx. Theoretical Arrhenius model / intrinsic material switching (DFT) overestimates the switching speed extracted from experiments.
Keywords: P1 Proceeding; Engineering sciences. Technology; Plasma Lab for Applications in Sustainability and Medicine – Antwerp (PLASMANT)
DOI: 10.1109/IEDM13553.2020.9372117