“TEM and AES investigations of the natural surface nano-oxide layer of an AISI 316L stainless steel microfibre”. Ramachandran D, Egoavil R, Crabbe A, Hauffman T, Abakumov A, Verbeeck J, Vandendael I, Terryn H, Schryvers D, Journal of microscopy 264, 207 (2016). http://doi.org/10.1111/jmi.12434
Abstract: The chemical composition, nanostructure and electronic structure of nanosized oxide scales naturally formed on the surface of AISI 316L stainless steel microfibres used for strengthening of composite materials have been characterised using a combination of scanning and transmission electron microscopy with energy-dispersive X-ray, electron energy loss and Auger spectroscopy. The analysis reveals the presence of three sublayers within the total surface oxide scale of 5.0-6.7 nm thick: an outer oxide layer rich in a mixture of FeO.Fe2 O3 , an intermediate layer rich in Cr2 O3 with a mixture of FeO.Fe2 O3 and an inner oxide layer rich in nickel.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 1.692
Times cited: 12
DOI: 10.1111/jmi.12434
|
|
|
“Melamine–Formaldehyde Microcapsules: Micro- and Nanostructural Characterization with Electron Microscopy”. Heidari H, Rivero G, Idrissi H, Ramachandran D, Cakir S, Egoavil R, Kurttepeli M, Crabbé, AC, Hauffman T, Terryn H, Du Prez F, Schryvers D, Microscopy and microanalysis 22, 1222 (2016). http://doi.org/10.1017/S1431927616012484
Abstract: A systematic study has been carried out to compare the surface morphology, shell thickness, mechanical properties, and binding behavior of melamine–formaldehyde microcapsules of 5–30 μm diameter size with various amounts of core content by using scanning and transmission electron microscopy including electron tomography, in situ nanomechanical tensile testing, and electron energy-loss spectroscopy. It is found that porosities are present on the outside surface of the capsule shell, but not on the inner surface of the shell. Nanomechanical tensile tests on the capsule shells reveal that Young’s modulus of the shell material is higher than that of bulk melamine–formaldehyde and that the shells exhibit a larger fracture strain compared with the bulk. Core-loss elemental analysis of microcapsules embedded in epoxy indicates that during the curing process, the microcapsule-matrix interface remains uniform and the epoxy matrix penetrates into the surface micro-porosities of the capsule shells.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 1.891
Times cited: 2
DOI: 10.1017/S1431927616012484
|
|