“A field study of the effectiveness of sacrificial anodes in ballast tanks of merchant ships”. De Baere K, Verstraelen H, Lemmens L, Lenaerts S, Dewil R, Van Ingelgem Y, Potters G, Journal of marine science and technology 19, 116 (2014). http://doi.org/10.1007/S00773-013-0232-3
Abstract: Sacrificial anodes have become a standard practice for the protection of ballast tanks of merchant vessels against corrosive damage. A well protected tank should extend the life span of a ship and consequently enhances its economic value. An in situ survey comprising more than 100 merchant vessels provided the opportunity to measure the impact of these anodes on the life expectancy of these vessels. Contrary to the general belief of these anodes beneficial effect, no significant difference was found in our observations in terms of corrosion occurrence between ship populations with and without sacrificial anodes, across all ship ages. This may be explained by the highly variable conditions and the complex geometry in a ballast tank severely impede optimal and straightforward installation of these anodes in these tanks. Also, poorly placed anodes in it may harm the integrity of the coating of the tank. We therefore plead for uniform and clear rules on anode installation and inspection.
Keywords: A1 Journal article; Engineering sciences. Technology; Sustainable Energy, Air and Water Technology (DuEL)
Impact Factor: 0.838
Times cited: 3
DOI: 10.1007/S00773-013-0232-3
|
|
|
“Analyzing the dispersion of cargo vapors around a ship’s superstructure by means of wind tunnel experiments”. Jacobs W, Reynaerts C, Andries S, van den Akker S, Moonen N, Lamoen D, Journal of marine science and technology 21, 758 (2016). http://doi.org/10.1007/s00773-016-0387-9
Abstract: In a previous study, it was found that cargo tank operations like cleaning and venting, lead to higher cargo vapor concentrations around the ship’s superstructure. Can wind tunnel experiments confirm these findings? Is there an improvement when using higher outlets at high velocities compared to lower outlets with a low outlet velocity? Is there a relation between relative wind speed and measured concentration? These questions were investigated in the Peutz wind tunnel. By using a tracer gas for the wind tunnel experiments, concentration coefficients have been calculated for various settings. The study shows that using high-velocity outlets is an efficient way to keep concentrations as low as possible. The only exception is for relative wind directions from the bow. In this last case using a manhole as ventilation outlet leads to lower concentrations. With increasing wind speeds the building downwash effect resulted in higher concentration coefficients near the main deck. This study confirms our on-board measurements and suggests the lowering of the ventilation inlet of the accommodation, so that the high-velocity outlet can be used safely at all times.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 0.838
Times cited: 2
DOI: 10.1007/s00773-016-0387-9
|
|
|
“Assessment of corrosion resistance, material properties, and weldability of alloyed steel for ballast tanks”. De Baere K, Verstraelen H, Willemen R, Smet J-P, Tchuindjang JT, Lecomte-Beckers J, Lenaerts S, Meskens R, Jung HG, Potters G, Journal of marine science and technology 22, 176 (2017). http://doi.org/10.1007/S00773-016-0402-1
Abstract: Ballast tanks are of great importance in the lifetime of modern merchant ships. Making a ballast tank less susceptible to corrosion can, therefore, prolong the useful life of a ship and, thereby, lower its operational cost. An option to reinforce a ballast tank is to construct it out of a corrosion-resistant steel type. Such steel was recently produced by POSCO Ltd., South Korea. After 6 months of permanent immersion, the average corrosion rate of A and AH steel (31 samples) was 535 g m(-2) year(-1), while the Korean CRS was corroding with 378 g m(-2) year(-1). This entails a gain of 29 %. Follow-up measurements after 10, 20, and 24 months confirmed this. The results after 6 months exposure to alternating wet/dry conditions are even more explicit. Furthermore, the physical and metallurgical properties of this steel show a density of 7.646 t/m(3), the elasticity modulus 209.3 GPa, the tensile strength 572 MPa, and the hardness 169HV10. Microscopically, the metal consists of equiaxed and recrystallized grains (ferrite and pearlite), with an average size of between 20 and 30 A mu m (ASTM E 112-12 grain size number between 7 and 8) with a few elongated pearlitic grains. The structure is banded ferrite/pearlite. On the basis of a series of energy dispersive X-ray spectrometer measurements the lower corrosion rate of the steel can be attributed to the interplay of Al, Cr, their oxides, and the corroding steel. In addition, the role of each element in the formation of oxide layers and the mechanisms contributing to the corrosion resistance are discussed.
Keywords: A1 Journal article; Sustainable Energy, Air and Water Technology (DuEL)
Impact Factor: 0.838
Times cited: 3
DOI: 10.1007/S00773-016-0402-1
|
|