“Gaining new insight into low-temperature aqueous photochemical solution deposited ferroelectric PbTiO3 films”. De Dobbelaere C, Lourdes Calzada M, Bretos I, Jimenez R, Ricote J, Hadermann J, Hardy A, Van Bael MK, Materials chemistry and physics 174, 28 (2016). http://doi.org/10.1016/J.MATCHEMPHYS.2016.02.047
Abstract: The nature of the low-temperature photochemical assisted formation process of ferroelectric lead titanate (PbTiO3) films is studied in the present work. Films are obtained by the deposition of an aqueous solution containing citric acid based (citrato) metal ion complexes with intrinsic UV activity. This UV activity is crucial for the aqueous photochemical solution deposition (aqueous PCSD) route being used. UV irradiation enhances the early decomposition of organics and results in improved electrical properties for the crystalline oxide film, even if the film is crystallized at low temperature. GATR-FTIR shows that UV irradiation promotes the decomposition of organic precursor components, resulting in homogeneous films if applied in the right temperature window during film processing. The organic content, morphology and crystallinity of the irradiated films, achieved at different processing atmospheres and temperatures, is studied and eventually correlated to the functional behavior of the obtained films. This is an important issue, as crystalline films obtained at low temperatures often lack ferroelectric responses. In this work, the film prepared in pure oxygen at the very low temperature of 400 degrees C and after an optimized UV treatment presents a significant remanent polarization value of P-r = 8.8 mu C cm(-2). This value is attributed to the better crystallinity, the larger grain size and the reduced porosity obtained thanks to the early film crystallization effectively achieved through the UV treatment in oxygen. (C) 2016 Elsevier B.V. All rights reserved.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 2.084
Times cited: 4
DOI: 10.1016/J.MATCHEMPHYS.2016.02.047
|
“Factors Influencing the Conductivity of Aqueous Sol(ution)-Gel-Processed Al-Doped ZnO Films”. Damm H, Adriaensens P, De Dobbelaere C, Capon B, Elen K, Drijkoningen J, Conings B, Manca JV, D’Haen J, Detavernier C, Magusin PCMM, Hadermann J, Hardy A, Van Bael MK;, Chemistry of materials 26, 5839 (2014). http://doi.org/10.1021/cm501820a
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 9.466
Times cited: 24
DOI: 10.1021/cm501820a
|
“Thermal decomposition synthesis of Al-doped ZnO nanoparticles : an in-depth study”. Damm H, Kelchtermans A, Bertha A, Van den Broeck F, Elen K, Martins JC, Carleer R, D'Haen J, De Dobbelaere C, Hadermann J, Hardy A, Van Bael MK;, RSC advances 3, 23745 (2013). http://doi.org/10.1039/c3ra43328e
Abstract: Al-doped ZnO nanoparticles are synthesized by means of a heating up solution based thermal decomposition method. The synthesis involves a reaction of zinc acetylacetonate hydrate, aluminium acetylacetonate and 1,2-hexadecanediol in the presence of oleic acid and oleyl amine. A proposed reaction mechanism from reagents to monomers is corroborated by analysis of the evolving gases using headspace GC-MS analysis. The Al-doped ZnO nanoparticles synthesized are dynamically stabilized by adsorbed oleate ions, after deprotonation of oleic acid by oleyl amine, as was found by NOESY proton NMR and complementary FTIR spectroscopy. Precession electron diffraction shows a simultaneous increase in lattice parameters with Al concentration. This, together with HAADF-STEM and EDX maps, indicates the incorporation of Al into the ZnO nanoparticles. By the combination of complementary characterization methods during all stages of the synthesis, it is concluded that Al is incorporated into the ZnO wurtzite lattice as a dopant.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 3.108
Times cited: 10
DOI: 10.1039/c3ra43328e
|
“Crystal structure and magnetic properties of the Cr-doped spiral antiferromagnet BiMnFe2O6”. Batuk D, de Dobbelaere C, Tsirlin AA, Abakumov AM, Hardy A, van Bael MK, Greenblatt M, Hadermann J, Materials research bulletin 48, 2993 (2013). http://doi.org/10.1016/j.materresbull.2013.04.038
Abstract: We report the Cr3+ for Mn3+ substitution in the BiMnFe2O6 structure. The BiCrxMn1-xFe2O6 solid solution is obtained by the solution-gel synthesis technique for the x values up to 0.3. The crystal structure investigation using a combination of X-ray powder diffraction and transmission electron microscopy demonstrates that the compounds retain the parent BiMnFe2O6 structure (for x = 0.3, a = 5.02010(6)angstrom, b = 7.06594(7)angstrom, c = 12.6174(1)angstrom, S.G. Pbcm, R-1 = 0.036, R-p = 0.011) with only a slight decrease in the cell parameters associated with the Cr3+ for Mn3+ substitution. Magnetic susceptibility measurements suggest strong similarities in the magnetic behavior of BiCrxMn1-xFe2O6 (x = 0.2; 0.3) and parent BiMnFe2O6. Only T-N slightly decreases upon Cr doping that indicates a very subtle influence of Cr3+ cations on the magnetic properties at the available substitution rates. (C) 2013 Elsevier Ltd. All rights reserved.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 2.446
Times cited: 3
DOI: 10.1016/j.materresbull.2013.04.038
|
“Analytical TEM study of CVD diamond growth on TiO2 sol-gel layers”. Lu Y-G, Verbeeck J, Turner S, Hardy A, Janssens SD, De Dobbelaere C, Wagner P, Van Bael MK, Van Tendeloo G, Diamond and related materials 23, 93 (2012). http://doi.org/10.1016/j.diamond.2012.01.022
Abstract: The early growth stages of chemical vapor deposition (CVD) diamond on a solgel TiO2 film with buried ultra dispersed diamond seeds (UDD) have been studied. In order to investigate the diamond growth mechanism and understand the role of the TiO2 layer in the growth process, high resolution transmission electron microscopy (HRTEM), energy-filtered TEM and electron energy loss spectroscopy (EELS) techniques were applied to cross sectional diamond film samples. We find evidence for the formation of TiC crystallites inside the TiO2 layer at different diamond growth stages. However, there is no evidence that diamond nucleation starts from these crystallites. Carbon diffusion into the TiO2 layer and the chemical bonding state of carbon (sp2/sp3) were both extensively investigated. We provide evidence that carbon diffuses through the TiO2 layer and that the diamond seeds partially convert to amorphous carbon during growth. This carbon diffusion and diamond to amorphous carbon conversion make the seed areas below the TiO2 layer grow and bend the TiO2 layer upwards to form the nucleation center of the diamond film. In some of the protuberances a core of diamond seed remains, covered by amorphous carbon. It is however unlikely that the remaining seeds are still active during the growth process.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 2.561
Times cited: 16
DOI: 10.1016/j.diamond.2012.01.022
|
“Properties and thermal stability of solution processed ultrathin, high-k bismuth titanate (Bi2Ti2O7) films”. Hardy A, Van Elshocht S, De Dobbelaere C, Hadermann J, Pourtois G, De Gendt S, Afanas'ev VV, Van Bael MK, Materials research bulletin 47, 511 (2012). http://doi.org/10.1016/j.materresbull.2012.01.001
Abstract: Ultrathin bismuth titanate films (Bi2Ti2O7, 5-25 nm) are deposited onto SiO2/Si substrates by aqueous chemical solution deposition and their evolution during annealing is studied. The films crystallize into a preferentially oriented, pure pyrochlore phase between 500 and 700 degrees C, depending on the film thickness and the total thermal budget. Crystallization causes a strong increase of surface roughness compared to amorphous films. An increase of the interfacial layer thickness is observed after anneal at 600 degrees C, together with intermixing of bismuth with the substrate as shown by TEM-EDX. The band gap was determined to be similar to 3 eV from photoconductivity measurements and high dielectric constants between 30 and 130 were determined from capacitance voltage measurements, depending on the processing conditions. (C) 2012 Elsevier Ltd. All rights reserved.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT); Plasma Lab for Applications in Sustainability and Medicine – Antwerp (PLASMANT)
Impact Factor: 2.446
DOI: 10.1016/j.materresbull.2012.01.001
|