“Synchrotron XRF analysis identifies cerium accumulation colocalized with pharyngeal deformities in CeO₂, NP-exposed caenorhabditis elegans”. Rossbach LM, Brede DA, Nuyts G, Cagno S, Olsson RMS, Oughton DH, Falkenberg G, Janssens K, Lind OC, Environmental science and technology 56, 5081 (2022). http://doi.org/10.1021/ACS.EST.1C08509
Abstract: A combination of synchrotron radiation-based elementalimaging, in vivo redox status analysis, histology, and toxic responses was usedto investigate the uptake, biodistribution, and adverse effects of Cenanoparticles (CeO2NP; 10 nm; 0.5-34.96 mg Ce L-1) or Ce(NO3)3(2.3-26 mg Ce L-1)inCaenorhabditis elegans. Elemental mapping of theexposed nematodes revealed Ce uptake in the alimentary canal prior todepuration. Retention of CeO2NPs was low compared to that of Ce(NO3)3in depurated individuals. X-rayfluorescence (XRF) mapping showed that Cetranslocation was confined to the pharyngeal valve and foregut. Ce(NO3)3exposure significantly decreased growth, fertility, and reproduction, causedslightly reduced fecundity. XRF mapping and histological analysis revealedsevere tissue deformities colocalized with retained Ce surrounding thepharyngeal valve. Both forms of Ce activated the sod-1 antioxidant defense,particularly in the pharynx, whereas no significant effects on the cellular redox balance were identified. The CeO2NP-induceddeformities did not appear to impair the pharyngeal function or feeding ability as growth effects were restricted to Ce(NO3)3exposure. The results demonstrate the utility of integrated submicron-resolution SR-based XRF elemental mapping of tissue-specificdistribution and adverse effect analysis to obtain robust toxicological evaluations of metal-containing contaminants.
Keywords: A1 Journal article; Antwerp X-ray Imaging and Spectroscopy (AXIS)
Impact Factor: 11.4
DOI: 10.1021/ACS.EST.1C08509
|
“All crystal clear : 18th-century glass à, la façon de Bohème from the cistercian nunnery of Clairefontaine, Belgium”. Herremans D, Cagno S, Vincke A, Janssens K, De Clercq W, Journal of glass studies 55, 137 (2013)
Abstract: Excavations at the Cistercian nunnery of Clairefontaine, located near Arlon in the south of Belgium, revealed an assemblage of 18th-century colorless glass. The morphology of the vessels and the engraved decoration suggest a central European origin or, at least, stylistic inspiration. The composition of the glass points to a recipe combining silica, lime, and potash: a colorless potash glass a la facon de Boheme. This article considers the technology, morphology, and origin of the vessels. The art-historical analysis is supported by chemical research (scanning electron microscopy energy-dispersive X-ray spectroscopy [SEM-EDX]). The finds are also discussed in light of the emerging northwestern European glass industry, changing consumer practices during the 18th century, and their meaning for the inhabitants of the abbey.
Keywords: A1 Journal article; Art; History; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
|
“The browning of stained glass windows : characterization of Mn-corrosion bodies and evaluation of cleaning methods”. Cagno S, Nuyts G, De Vis K, Caen J, Van Mol W, Bongaers E, Pauwels B, Janssens K, (2011)
Keywords: P3 Proceeding; Engineering sciences. Technology; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
|
“Characterization of 18th century Portuguese glass from Real Fábrica de Vidros de Coina”. Lopes F, Lima A, Pires de Matos A, Custódio J, Cagno S, Schalm O, Janssens K, Journal of Archaeological Science: Reports 14, 137 (2017). http://doi.org/10.1016/J.JASREP.2017.05.020
Abstract: This work reports the first systematic chemical characterization of Portuguese 18th century glassware. 28 selected glass fragments, recovered from an archaeological excavation carried out in the site where King D. João V of Portugal established an important glass manufacture, Real Fábrica de Vidros de Coina (Coina Royal Glass Factory), were studied. This factory operated from 1719 until 1747, the year in which the factory was transferred to Marinha Grande. The fragments were analysed by micro-energy dispersive X-ray fluorescence (micro-EDXRF), using a portable spectrometer ArtTAX, and scanning electron microscopy (SEM-EDX). The analytical data showed that a large variety of glass types was manufactured in that factory, namely soda-lime glass, mixed-alkali glass, high lime-low alkali glass, potash glass and lead glass. In general, the composition of the glass varies according to the function of the objects. It was demonstrated that micro-EDXRF can be an important tool to characterize museum glass objects when only in situ non-invasive analytical methods are allowed.
Keywords: A1 Journal article; Engineering sciences. Technology; Art; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation); Antwerp Cultural Heritage Sciences (ARCHES)
Times cited: 3
DOI: 10.1016/J.JASREP.2017.05.020
|
“Combined computed nanotomography and nanoscopic x-ray fluorescence imaging of cobalt nanoparticles in caenorhabditis elegans”. Cagno S, Brede DA, Nuyts G, Vanmeert F, Pacureanu A, Tucoulou R, Cloetens P, Falkenberg G, Janssens K, Salbu B, Lind OC, Analytical chemistry 89, 11435 (2017). http://doi.org/10.1021/ACS.ANALCHEM.7B02554
Abstract: Synchrotron radiation phase-contrast computed nanotomography (nano-CT) and two-and three-dimensional (2D and 3D) nanoscopic X-ray fluorescence (nano-XRF) were used to investigate the internal distribution of engineered-cobalt nanoparticles (Co NPs) in exposed individuals of the nematode Caenorhabditis elegans. Whole-nematodes and selected tissues and organs were 3D-rendered: anatomical 3D renderings with 50 nm voxel size enabled the visualization of spherical nanoparticle aggregates. with size tip to 200 nm within intact C. elegans. A 20 X 37 nm(2) high-brilliance beam was employed to obtain XRF elemental distribution maps of entire nematodes or anatomical details such as embryos, which could be compared with the CT data, These maps showed Co NPs to be predominantly present within the intestine and the epithelium, and they were not colocalized with Zn granules found in the lysosonie-containing vesicles or Fe agglomerates in the intestine. Iterated XRF scanning of a specimen at 0 degrees and 90 degrees angles suggested that NP aggregates were translocated into tissues outside of the intestinal lumen. Virtual-slicing by means of 2D XRF tomography, combined with holotomography, indicated presumable presence of individual NP aggregates inside the uterus and within embryos.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 6.32
Times cited: 13
DOI: 10.1021/ACS.ANALCHEM.7B02554
|
“Composition and state of alteration of 18th-century glass finds found at the Cistercian nunnery of Clairefontaine, Belgium”. Hellemans K, Vincke A, Cagno S, Herremans D, De Clercq W, Janssens K, Journal of archaeological science 47, 121 (2014). http://doi.org/10.1016/J.JAS.2014.03.039
Abstract: A hundred 18th-century glass fragments were recovered at the Clairefontaine monastery in the Belgian province of Luxembourg. They were analysed by a combination of SEM-EDX and LA-ICP-MS in order to determine their major composition as well as their trace element signature. Multivariate statistical methods such as hierarchical clustering and principal component analysis were used to divide the glass fragments into four main groups: potassium-rich glass, sodium-rich glass, potassium/lime-rich glass and high-lime-low-alkali glass. Within every group, not only a similarity in composition is observed, but also in colour, morphology and deterioration patterns. Potash glass fragments are the most abundant and show extensive deterioration; two classes of potash glass were identified: one similar to certain Central European glass compositions, while the other one, characterised by large variations in potash: lime ratio, may be attributed to local (regional) glass production. (C) 2014 Elsevier Ltd. All rights reserved.
Keywords: A1 Journal article; Philosophy; History; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 2.602
Times cited: 12
DOI: 10.1016/J.JAS.2014.03.039
|
“Composition and state of alteration of 18th century glass from the Cistercian nunnery of Clairefontaine (Belgium)”. Herremans D, Cagno S, Vincke A, de Clercq W, Janssens K, Proceedings of the Society of Photo-optical Instrumentation Engineers
T2 –, Conference on Integrated Approaches to the Study of Historical Glass, (IASHG), APR 16-17, 2012, Brussels, BELGIUM , 842206 (2012). http://doi.org/10.1117/12.975247
Abstract: An extended set of 18th century glass vessels was analyzed by means of SEM-EDX (major and minor element composition) The fragmented archaeological objects were recovered from a latrine belonging to the early 18th century building phase of the nunnery of Clairefontaine, near Arlon (B). On the basis of typology and decoration, the major part of the vessels could be dated around the middle of the 18th century. Variety in color and weathering of the glass suggest differences in glassmaking recipes and in the composition and origin of raw materials. The results of the analysis show how two main compositional groups constitute about 90% of the analyzed glass set, and these are constituted by potash glass (transparent beakers) and high lime low alkali glass (green bottles). Next to these, a few potash-lime and soda glasses are also found. The type of alteration has also a clear relation with the original glass composition.
Keywords: P1 Proceeding; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
DOI: 10.1117/12.975247
|
“Composition of Facon de Venise glass from early 17th century London in comparison with luxury glass of the same age”. Cagno S, de Raedt I, Jeffries T, Janssens K, Proceedings of the Society of Photo-optical Instrumentation Engineers
T2 –, Conference on Integrated Approaches to the Study of Historical Glass, (IASHG), APR 16-17, 2012, Brussels, BELGIUM , 842205 (2012). http://doi.org/10.1117/12.975212
Abstract: SEM-EDX and LA-ICP-MS analyses were performed on a set of early 17th century London glass fragments. The samples originate from two archaeological sites (Aldgate and Old Broad Street) where glass workshops were active in this period. The great majority of the samples are made of soda glass. Two distinct compositional groups are observed, each typical of one site of provenance. The samples originating from the Old Broad Street excavation feature a silica-soda-lime composition, with a moderate amount of potash. The samples from Aldgate are richer in potassium and feature higher amounts of trace elements such as Rb, Zr and Cu. The distinction between the two groups stems from different flux and silica sources used for glassmaking. A comparison with different European glass compositions of that time reveals no resemblance with genuine Venetian production, yet the composition of the Old Broad Street glass shows a close similarity to that of fragments produced 'a la facon de Venise' in Antwerp at the end of the 16th century. This coincides with historical sources attesting the arrival of glassworkers from the Low Countries in England and suggests that a transfer of technology took place near the turn of the century.
Keywords: P1 Proceeding; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Times cited: 1
DOI: 10.1117/12.975212
|
“Compositional analysis of Tuscan glass samples: in search of raw materials fingerprints”. Cagno S, Janssens K, Mendera M, Analytical and bioanalytical chemistry 391, 1389 (2008). http://doi.org/10.1007/S00216-008-1945-8
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 3.431
Times cited: 26
DOI: 10.1007/S00216-008-1945-8
|
De Vis K, Cagno S, Van Mol W, Schalm O, Janssens K, Caen J (2012) The decolourization of manganese-stained glass : the conversion reaction and evaluation of its effectiveness. 463–468
Keywords: P2 Proceeding; Engineering sciences. Technology; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
|
“Deeply colored and black-appearing Roman glass : a continued research”. Cagno S, Cosyns P, Izmer A, Vanhaecke F, Nys K, Janssens K, Journal of archaeological science 42, 128 (2014). http://doi.org/10.1016/J.JAS.2013.11.003
Abstract: In the context of archaeological and historical assessment of Roman black-appearing glass, the chemical and physical characterization of a large collection of samples originating from various areas of the Roman Empire has been gathered over the past years to (i) verify whether a minor segment of the overall Roman glass production can help in determining possible diachronic changes in Roman imperial glass production (1st century AD – 5th century AD) and (ii) reveal regional compositional differences. In this paper, the latest results on the chemical composition of an additional 44 black-appearing Roman glass samples are presented, together with general conclusions based upon the entire compositional dataset of over 400 analyzed black glass samples. The results show that the Roman black glass is obtained through several glass compositions with a specific chronological, geographical and typological distribution. (C) 2013 Elsevier Ltd. All rights reserved.
Keywords: A1 Journal article; Philosophy; History; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 2.602
Times cited: 18
DOI: 10.1016/J.JAS.2013.11.003
|
“Deeply coloured and black glass in the Northern provinces of the Roman Empire : differences and similarities in chemical composition before and after AD 150”. van der Linden V, Cosyns P, Schalm O, Cagno S, Nys K, Janssens K, Nowak A, Wagner B, Bulska E, Archaeometry 51, 822 (2009). http://doi.org/10.1111/J.1475-4754.2008.00434.X
Abstract: In this work we attempt to elucidate the chronological and geographical origin of deeply coloured and black glass dating between 100 bc and ad 300 on the basis of their major and trace element compositions. Samples from the western and eastern parts of the Roman Empire were analysed. Analytical data were obtained by means of a scanning electron microscope – energy-dispersive system (SEM-EDS, 63 samples analysed) and laser ablation – inductively coupled plasma – mass spectrometry (LA-ICP-MS, 41 samples analysed). Among the glass fragments analysed, dark brown, dark purple and dark green hues could be distinguished. Only among the dark green fragments could a clear compositional distinction be observed between fragments dated to the periods before and after ad 150. In the early samples (first century bc to first century ad), iron, responsible for the green hue, was introduced by using impure sand containing relatively high amounts of Ti. In contrast, a Ti-poor source of iron was employed, containing Sb, Co and Pb in trace quantities, in order to obtain the dark green colour in the later glass samples. The analytical results obtained by combining SEM-EDS and LA-ICP-MS are therefore consistent with a differentiation of glassmaking recipes, detectable in glass composition, occurring in the period around ad 150.
Keywords: A1 Journal article; History; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 1.47
Times cited: 39
DOI: 10.1111/J.1475-4754.2008.00434.X
|
“Evaluation of manganese-bodies removal in historical stained glass windows via SR-\mu-XANES/XRF and SR-\mu-CT”. Cagno S, Nuyts G, Bugani S, De Vis K, Schalm O, Caen J, Helfen L, Cotte M, Reischig P, Janssens K, Journal of analytical atomic spectrometry 26, 2442 (2011). http://doi.org/10.1039/C1JA10204D
Abstract: The speed and effectiveness of a conservation treatment used for stained glass windows have been investigated. Dark-coloured Mn-rich stains can be found in the alteration layer of ancient glass artefacts and cause the surface to turn brown/black: this phenomenon is known as Mn-browning or Mn-staining. While in glass manganese is present in the +II or +III oxidation states, in the Mn-rich bodies, manganese is in a higher oxidation state (+IV). In restoration practice, mildly reducing solutions are employed to eliminate the dark colour and restore the clear appearance of the glass. In this paper the effectiveness and side effects of the use of hydroxylamine hydrochloride for this purpose are assessed. Archaeological fragments of stained glass windows, dated to the 14th century and originating from Sidney Sussex College, Cambridge (UK), were examined by means of synchrotron radiation (SR) based microscopic X-ray Absorption Near-Edge Spectroscopy (μ-XANES) and microscopic X-Ray Fluorescence (μ-XRF) and with high resolution computed absorption tomography (μ-CT) before, during and after the treatment. The monitoring of the glass fragments during the treatment allows us to better understand the manner in which the process unfolds and its kinetics. The results obtained reveal that the hydroxylamine hydrochloride treatment is effective, but also that it has a number of unwanted side effects. These findings are useful for optimizing the time and other modalities of the Mn-reducing treatment as well as minimizing its unwanted results.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 3.379
Times cited: 17
DOI: 10.1039/C1JA10204D
|
“Evidence of early medieval soda ash glass in the archaeological site of San Genesio (Tuscany)”. Cagno S, Favaretto L, Mendera M, Izmer A, Vanhaecke F, Janssens K, Journal of archaeological science 39, 1540 (2012). http://doi.org/10.1016/J.JAS.2011.12.031
Abstract: The early medieval period marks an important turning point in the history of glassmaking, since it comprises the transition period between the mineral-based silica-soda-lime glass of the Roman tradition and the plant ash-based glass. With the aim of expanding the knowledge on the glass recipes and technologies of this period, 37 glass samples were analyzed, originating from the archaeological excavations of San Genesio (Tuscany) and dated from the fourth to the eleventh century. The major and minor element concentrations were measured with SEM-EDX, while the trace elements were quantified with LA-ICP-MS. The results were compared with published compositions of glass samples of similar age in order to highlight differences and similarities. The results offer a very interesting view on the glass circulation in the religious/residential/manufacturing center of San Genesio in the early medieval period. Most of the glass has a typical late-Roman composition, but some glass fragments are identified as soda ash glass. These are among the earliest medieval ash-fluxed glasses ever found in the Italian peninsula. (C) 2011 Elsevier Ltd. All rights reserved.
Keywords: A1 Journal article; Philosophy; History; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 2.602
Times cited: 24
DOI: 10.1016/J.JAS.2011.12.031
|
Bruijnen Y, Caen JMA, Cagno S, Janssens K, et al. (2012) Getekend Jan R. : Jan Rombouts, een renaissancemeester herontdekt. 207 p
Keywords: ME2 Book as editor or co-editor; Art; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
|
“High-resolution desktop microcomputed tomography for the evaluation of reducing treatments on historical glass suffering from manganese browning”. Nuyts G, Cagno S, Jaroszewicz J, Wouters H, De Vis K, Caen J, Janssens K page 201 (2013).
Abstract: Historical glass, especially non-durable mediaeval glass, can undergo corrosion. This sometimes results in the formation of dark-coloured manganese-rich inclusions or stains that reduce the transparency of the glass. A conservation treatment with reducing or chelating agents may be considered with the aim of improving the transparency. In this paper, high-resolution desktop microcomputed tomography (µCT) is used in combination with element-specific twodimensional imaging methods for in situ monitoring of manganese removal by hydroxylamine hydrochloride from an archaeological stained-glass sample suffering from manganese browning and from artificially corroded model glass samples. µCT also proved itself useful for the study of the (re-)penetration of manganese into the gel layer during artificial corrosion of a model glass.
Keywords: H2 Book chapter; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation); Antwerp Cultural Heritage Sciences (ARCHES)
|
“The identification of chromophores in ancient glass by the use of UV-VIS-NIR spectroscopy”. Meulebroeck W, Baert K, Wouters H, Cosyns P, Ceglia A, Cagno S, Janssens K, Nys K, Terryn H, Thienpont H, Proceedings of the Society of Photo-optical Instrumentation Engineers 7726, 77260d (2010). http://doi.org/10.1117/12.853666
Abstract: In this publication optical spectroscopy is considered to be a supplementary technique to study ancient colored glass. It results from a systematic study of the UV-VIS-NIR transmission spectra of intentionally colored glass fragments from various archaeological and historical sites and dated from the Roman period to the 21th century AD. The main goal consists of defining optical sensing parameters for this type of material. The considered colorants are iron, cobalt, manganese, copper and chromium. It is proved that many cases exist where optical spectroscopy can be seen as a straightforward, non-destructive, low-cost and in-situ applicable technique in identifying authentic material or to obtain information about the origin of the material. Possible sensing parameters are defined as the absence/presence of absorption bands characteristic for a specific coloring metal oxide and the spectral position of these bands. These parameters could reveal information about the applied furnace conditions and/or to the composition of the glass matrix. It is shown that the cobalt absorption band situated around 535 nm for soda rich glasses (Roman and industrial times) is shifted towards 526 nm for potash rich glasses (medieval and post-medieval times).
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Times cited: 10
DOI: 10.1117/12.853666
|
“Iron speciation in soda-lime-silica glass: a comparison of XANES and UV-vis-NIR spectroscopy”. Ceglia A, Nuyts G, Meulebroeck W, Cagno S, Silvestri A, Zoleo A, Nys K, Janssens K, Thienpont H, Terryn H, Journal of analytical atomic spectrometry 30, 1552 (2015). http://doi.org/10.1039/C5JA00046G
Abstract: Scientific analyses of ancient glasses have been carried out for many years using elemental chemical analysis. However, it is known that the control of the redox conditions in the glass melt has a strong implication on the final hue of glass because it affects Fe2+/SFe. Therefore an increasing number of studies on the redox conditions have been published in recent years by means of synchrotron based Xray absorption spectroscopy. This is a technique which is not easily accessible and requires dedicated facilities. In this paper we describe an alternative approach by means of optical absorption spectroscopy. We synthesised 10 soda-lime-silica glasses with known redox conditions and iron concentration to calibrate the absorption at 1100 nm as a function of Fe2+ concentration. The linear extinction coefficient was also determined. These glasses were also studied by means of X-ray Absorption Near Edge Structure (XANES) spectroscopy. Electron paramagnetic resonance spectroscopy was additionally used as an ancillary method to verify the quality of our data. Furthermore 28 samples from real archaeological samples were analysed by XANES and optical spectroscopy as a case study. The Fe2+/SFe values obtained were compared and demonstrated that the two techniques were in good agreement with each other. Optical spectroscopy can be applied in situ with moderate sample preparation to determine the concentration of Fe2+. To investigate the redox conditions, especially as a first screening approach, this methodology is an important tool to take into consideration before applying more sophisticated techniques such as XANES, which is more elaborate and requires high-tech resources.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 3.379
Times cited: 20
DOI: 10.1039/C5JA00046G
|
“LA-ICP-MS for Pu source identification at Mayak PA, the Urals, Russia”. Cagno S, Hellemans K, Lind OC, Skipperud L, Janssens K, Salbu B, Environmental science : processes &, impacts 16, 306 (2014). http://doi.org/10.1039/C3EM00531C
Abstract: Information on Pu in environmental samples is traditionally based on the determination of the 240+239PU activity via Alpha Spectrometry (AS). A large number of alpha spectrometry sources (planchettes) containing radiochemically separated Pu are therefore stored worldwide and are available for further analyses. These archive samples represent a resource from which valuable information on isotopic composition of alpha emitters including Pu can be obtained. The relative abundances of Pu isotopes can be used to trace specific Pu sources and characterize the relative contributions of different Pu sources in a sample. Thus, in addition to the total 239+240PU activity, determination of the Pu-240/Pu-239 ratio can provide valuable information on the nature of the Pu emitting sources. The Pu isotopic ratios can be determined by mass spectrometry techniques such as Sector Field Inductively Coupled Plasma Mass Spectrometry (SF-ICPMS) or Accelerator Mass Spectrometry (AMS) that require dissolution and complete destruction of the material deposited on the planchettes. In this study Laser Ablation (LA)-quadrupole-ICP-MS has been employed for the analysis of Pu-239/Pu-240 ratios from alpha-planchettes prepared from samples originating from the Mayak PA nuclear facility, Russia. The results are compared with data from AMS and show that the Pu-240/Pu-239 ratios obtained by LA-ICP-MS can be utilized to distinguish weapons-grade Pu from civil reprocessing sources. Moreover, isotope ratio mapping can also be performed across the planchettes, allowing e.g. the visualization of possible inhomogeneities in the Pu-isotope distribution on their surface. Thus, this solid sample technique can be applied to extract additional information from existing archives of samples.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 2.592
Times cited: 10
DOI: 10.1039/C3EM00531C
|
“LA-ICP-MS labels early medieval Tuscan finds from Siena and Donoratico as late natron glass”. Hellemans K, Cagno S, Bogana L, Janssens K, Mendera M, Journal of Archaeological Science: Reports 23, 844 (2019). http://doi.org/10.1016/J.JASREP.2018.12.002
Abstract: The late antique/early medieval age in Central Italy is a well-suited context to verify the implications of the end of the natron glass supplies, and to explore the beginnings of the new plant-ash glass technology. We present the results of a LA-ICP-MS analysis campaign conducted on archaeological glass finds excavated at the Santa Maria della Scala hospital site in Siena and in Donoratico. This provided us with major, minor and trace element quantitative data for 49 glass samples belonging to drinking vessels and lamps, dated mainly between the 5th and the 8th century. On the basis of these data, we have sought to identify the working processes and possible glassware trade that are reflected in the glass composition. Major and minor element contents revealed that most samples, also at the later boundary of the explored timeframe, fit well within known late Roman glass classifications (e.g. HIMT, Levantine). Trace element analysis provided further information on the raw materials that were used in the glassmaking process, indicating the use of coastal sands as a silica source and allowing us to formulate different hypotheses on the materials used for the colouring process.
Keywords: A1 Journal article; History; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Times cited: 3
DOI: 10.1016/J.JASREP.2018.12.002
|
“Manganese staining of archaeological glass : the characterization of Mn-rich inclusions in leached layers and a hypothesis of its formation”. Schalm O, Proost K, De Vis K, Cagno S, Janssens K, Mees F, Jacobs P, Caen J, Archaeometry 53, 103 (2011). http://doi.org/10.1111/J.1475-4754.2010.00534.X
Abstract: During the study of a large number of archaeological glass fragments, manganese-rich inclusions in leached layers were observed in a limited number of cases. This phenomenon occurs only in black-coloured leached layers. Since the formation mechanism of such manganese-rich inclusions is still unclear, a combination of several analytical techniques was used in order to investigate this phenomenon and, more specifically, to obtain more information on (a) the composition and morphology of the inclusions, (b) the chemical state of Mn and (c) the 3D morphology of the inclusions. A mechanism that might explain the formation of these inclusions is proposed.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 1.47
Times cited: 24
DOI: 10.1111/J.1475-4754.2010.00534.X
|
“Micro-XANES study on Mn browning: use of quantitative valence state maps”. Nuyts G, Cagno S, Bugani S, Janssens K, Journal of analytical atomic spectrometry 30, 642 (2015). http://doi.org/10.1039/C4JA00386A
Abstract: Historical glass, especially non-durable medieval glass, can undergo corrosion. This sometimes results in the formation of dark-coloured manganese-rich inclusions that reduce the transparency of the glass. While unaltered bulk glass contains manganese mainly present in the +II valence state, inside the inclusions Mn is present in higher valence states (+III to +IV). Two different strategies may be considered by conservators when aiming to improve the transparency. One is based on the reduction of highly oxidised black/brown compounds using mildly reducing solutions, while the other focuses more on the extraction of manganese from the inclusions by the application of chelating agents. In this paper, a method for quantitative mapping of the Mn speciation inside partially corroded historical windowpanes based on X-Ray Absorption Near-Edge Structure (XANES) spectroscopy is discussed. The calibration of such Mn valence state maps based on the combo method, a fairly reliable way to determine the oxidation state, is described in more detail. This method is used to evaluate the effect of reducing treatments on historical glass, dated to the 14th century and originating from Sidney Sussex College (Cambridge, UK), suffering from Mn browning. Glasses were examined by means of Synchrotron Radiation (SR) based microscopic X-Ray Absorption Near-Edge Structure (mXANES) spectroscopy and microscopic X-Ray Fluorescence (mXRF). X-Ray elemental distribution maps of glass cross-sections are recorded at different energies, while Mn K-edge spectra are used to convert these into Mn valence state (VS) maps. Such valence state maps will allow evaluation of a reducing treatment.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 3.379
Times cited: 8
DOI: 10.1039/C4JA00386A
|
“Optical spectroscopy as a rapid and low-cost tool for the first-line analysis of glass artefacts : a step-by-step plan for Roman green glass”. Meulebroeck W, Cosyns P, Baert K, Wouters H, Cagno S, Janssens K, Terryn H, Nys K, Thienpont H, Journal of archaeological science 38, 2387 (2011). http://doi.org/10.1016/J.JAS.2011.04.023
Abstract: Archaeometric research on glass artefacts is continuously evolving and is converging towards a multidisciplinary research domain where different types of techniques are applied depending on the questions asked and the circumstances involved. The technique described in this work is optical spectroscopy. The benefit of this technique being the possibility of building up a knowledge database for a large amount of material in a relatively short period of time and with a relatively limited budget. This is of particular interest for the investigation of extensive and/or unexplored glass collections where a first-line analysis of artefacts could facilitate the selection of material needing further and more detailed examination. This publication explores the extent to which optical spectroscopy can be used for a first-line analysis of green coloured glass artefacts from the Roman period. It is shown that the colour coordinates calculated from the measured transmission spectrum could reveal information about the fragment under study. In particular it is shown that 1) based on the position of the calculated colour values on the colour diagram (CIE1931) one could easily know whether the artefact was coloured using only iron or if copper oxides were also present. In the case of the artefact owing its colour solely to the presence of iron, the distance between the measured colour values and the colour diagrams white point can roughly indicate the iron concentration of the sample; 2) artefacts that were fabricated under similar furnace conditions can also be identified on the colour diagram; 3) samples with identical compositions and fabrication conditions but with different sample thickness, gave rise to a variation in the colour coordinates, thus allowing optical spectroscopy to help identify fragments which might belong to the same object.
Keywords: A1 Journal article; Engineering sciences. Technology; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 2.602
Times cited: 18
DOI: 10.1016/J.JAS.2011.04.023
|
“Raw materials for medieval to post-medieval Tuscan glassmaking : new insight from LA-ICP-MS analyses”. Cagno S, Mendera M, Jeffries T, Janssens K, Journal of archaeological science 37, 3030 (2010). http://doi.org/10.1016/J.JAS.2010.06.030
Abstract: LA-ICP-MS analyses were performed on a set of Tuscan (post) medieval archaeological glass finds dated to the 1316th century in order to quantitatively determine the trace element contents. The results are used for defining and distinguishing several compositional groups. The trace element data are consistent with the distinctions obtained by considering the major element data determined via quantitative SEM-EDX, but allow to obtain new insights into the nature and quality of the silica sources employed and the presumed method of ash purification.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 2.602
Times cited: 38
DOI: 10.1016/J.JAS.2010.06.030
|
“Revealing hidden paint layers in oil paintings by means of scanning macro-XRF : a mock-up study based on Rembrandt's “An old man in military costume””. Alfeld M, de Nolf W, Cagno S, Janssens K, et al, Journal of analytical atomic spectrometry 28, 40 (2013). http://doi.org/10.1039/C2JA30119A
Abstract: Over the past several decades the oeuvre of Rembrandt has been the subject of extensive art historical and scientific investigations. One of the most striking features to emerge is his frequent re-use of canvases and panels. The painting An Old Man in Military Costume (78.PB.246), in the collection of the J. Paul Getty Museum, is an example of such a re-used panel. Conventional imaging techniques revealed the presence of a second portrait under the surface portrait, but the details of this hidden portrait have not yet been revealed. Vermilion (HgS) has been identified to have been used nearly exclusively in the flesh tones of the lower painting, suggesting that element-specific XRF imaging might successfully image the hidden portrait. To test this hypothesis, a full-scale mock-up of the painting was created, including a “free impression” of the hidden portrait, reproducing as closely as possible the pigments and paint stratigraphy of the original painting. XRF imaging of the mock-up painting was conducted using three different XRF imaging systems: a mobile X-ray tube based system and two synchrotron-based setups (one equipped with multiple SDDs and one equipped with a Maia detector). The sensitivity, limits of detection and imaging capabilities of each system under the chosen experimental conditions are evaluated and compared. The results indicate that an investigation of the original painting by this method would have an excellent chance of success.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 3.379
DOI: 10.1039/C2JA30119A
|
“The stained-glass panel depicting the anointing at Bethany : art historical research, technical analysis, and treatment”. Caen J, Cagno S, Janssens K page 247 (2013).
Abstract: In 2008, Museum M in Louvain (Flanders, Belgium) acquired a panel depicting The Anointing at Bethany that is believed once to have adorned the citys former Charterhouse. The panel required conservation treatment, which was preceded by a thorough art-historical and technical examination. It emerged that comparable panels are kept at the Metropolitan Museum of Art and the Riverside Church in New York. Chemical analyses show most of the glass in the panel to have a typical 16th century high-limelow-alkali composition. The conservation treatment was based on the evaluation of these findings and focused very strongly on enhancing the aesthetic balance for an improved reading of the panel.
Keywords: H2 Book chapter; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation); Antwerp Cultural Heritage Sciences (ARCHES)
|
“Study of medieval glass fragments from Savona (Italy) and their relation with the glass produced in Altare”. Cagno S, Badano MB, Mathis F, Strivay D, Janssens K, Journal of archaeological science 39, 2191 (2012). http://doi.org/10.1016/J.JAS.2012.03.013
Abstract: Altare was in the medieval and post-medieval period an important glassmaking center in the Liguria region in Northern Italy. The first historical evidence of glassmaking in Altare is dated to the twelfth century. In spite of that, due to the continuity of glassmaking up to the present time and the contemporaneous intensive urbanization of the territory, no medieval glass from Altare or its immediate vicinity has been analyzed up to now. In this work, glass from archaeological excavations in the center of Savona, city with close ties with the glassmaking center, was studied. Glass fragments, dated from the tenth to the sixteenth century were selected from the collections of the Archaeological Museum in Savona and non-destructively analyzed with quantitative PIXE-PIGE. The resulting compositions, compared with known glass productions of the same time and evaluated on the basis of historical documents, offer an interesting panorama on the variety of glass circulation in Liguria. (C) 2012 Elsevier Ltd. All rights reserved.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 2.602
Times cited: 21
DOI: 10.1016/J.JAS.2012.03.013
|
“Study of the early stages of Mn intrusion in corroded glass by means of combined SR FTIR/\muXRF imaging and XANES spectroscopy”. Nuyts G, Cagno S, Hellemans K, Veronesi G, Cotte M, Janssens K, Procedia Chemistry
T2 –, Youth in Conservation of Cultural Heritage Conference (YOCOCU), June 18-20, 2012, University of Antwerp, Antwerp, Belgium , 239 (2013). http://doi.org/10.1016/J.PROCHE.2013.03.030
Abstract: Historical glass, especially medieval glass, can undergo weathering under the influence of time and environmental conditions. The aim of this investigation was to better understand the processes involved in this natural degradation process by studying artificially altered glass samples prepared for the use of evaluation of conservation methods. Non-durable glass sensors produced by the Fraunhofer Institute (type M1.0) were used as a starting material for artificial alteration. These were immersed in acidic (pH = 0, 2, 4) and neutral solutions (1 h – 8 h). In a second stage the glass samples were immersed in a 0.5 M MnCl2 solution (24 h, 48 h and 72 h), allowing intrusion of Mn from the solution into the gel layer. The samples were characterized at different stages with reflectance FTIR spectroscopy, mu XRF mapping and mu XANES. All measurements were carried out at ESRF, beamline ID21. Reflectance FTIR spectroscopy measurements were performed in the 800 4000 cm(-1) range. Cluster analysis of the resulting maps evidenced the rapid growth of the gel layer in strong acidic conditions. The average spectra for each cluster feature show for the original glass a strong Si-O- stretching band between 900 and 1000 cm(-1), whereas the gel layer could be identified by the increasing Si-O-Si bands around 1100 and 1250 cm(-1). mu XRF maps were recorded at different stages of the experiment at energies around the Mn-K edge (6.539 keV) and with a step size of 2 by 2 m. These confirm the leaching of K+ and Ca+2 from the glass and the intrusion of Mn from the solution. Mn was found throughout the entire gel layer, but with a concentration gradient peaking at the surface. XANES point measurements were recorded at various points where Mn was present. No spatial variation was found, but linear combination fitting of the spectra with various Mn reference compounds indicated that Mn2+Mn23+O4 is the main Mn compound in the gel layer, as was hypothesised by Watkinson et al. The standard corroded glass samples studied here can be used for the evaluation of conservation treatments in follow-up experiments. (C) 2013 The Authors. Published by Elsevier B.V. Selection and peer-review under responsibility of the IA-CS (Italian Association of Conservation Scientists) and University of Antwerp
Keywords: P1 Proceeding; Engineering sciences. Technology; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Times cited: 4
DOI: 10.1016/J.PROCHE.2013.03.030
|
“Study on the impregnation of archaeological waterlogged wood with consolidation treatments using synchrotron radiation microtomography”. Bugani S, Modugno F, Lucejko JJ, Giachi G, Cagno S, Cloetens P, Janssens K, Morselli L, Analytical and bioanalytical chemistry 395, 1977 (2009). http://doi.org/10.1007/S00216-009-3101-5
Abstract: In favourable conditions of low temperature and low oxygen concentration, archaeological waterlogged wooden artefacts, such as shipwrecks, can survive with a good state of preservation. Nevertheless, anaerobic bacteria can considerably degrade waterlogged wooden objects with a significant loss in polysaccharidic components. Due to these decay processes, wood porosity and water content increase under ageing. In such conditions, the conservation treatments of archaeological wooden artefacts often involve the replacement of water with substances which fill the cavities and help to prevent collapse and stress during drying. The treatments are very often expensive and technically difficult, and their effectiveness very much depends on the chemical and physical characteristics of the substances used for impregnation. Also important are the degree of cavity-filling, penetration depth and distribution in the structure of the wood. In this study, the distribution in wood cavities of some mixtures based on polyethylene glycols and colophony, used for the conservation of waterlogged archaeological wood, was investigated using synchrotron radiation X-ray computed microtomography (SR-A mu CT). This non-destructive imaging technique was useful for the study of the degraded waterlogged wood and enabled us to visualise the morphology of the wood and the distribution of the materials used in the wood treatments. The study has shown how deposition is strictly related to the dimension of the wooden cavities. The work is currently proceeding with the comparison of synchrotron observations with the data of the solutions viscosity and with those of the properties imparted to the wood by the treatments.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 3.431
Times cited: 30
DOI: 10.1007/S00216-009-3101-5
|
“The use of vitrum obsianum in the Roman Empire: some new insights and future prospects”. Cagno S, Cosyns P, Ceglia A, Nys K, Janssens K, Periodico di mineralogia 84, 465 (2015). http://doi.org/10.2451/2015PM0026
Abstract: The research on the use of obsidian in the Mediterranean is extensive but concerns almost exclusively volcanic glass from prehistoric and Bronze Age contexts. The consumption of obsidian during the Roman imperial period, however, has only occasionally received attention. Never a comprehensive account on what the Romans made in vitrum obsianum has been set up, nor have the sources exploited by them been examined. This paper provides a concise overview of the current knowledge on obsidian during the Roman imperial period and offers an introductory outline on potential research. The ancient writers inform us about the use of volcanic glass to create exclusive vessels, gemstones, mirrors and sculpture, but also about the creation of black appearing man-made glass initiated as a cheap and easier workable substitute of obsidian. The archaeological data on the other hand propose a more complex story with the occurrence of obsidian chunks in early Roman secondary glass workshops, and the bulky use of obsidian in late Antiquity to produce tesserae for the creation of wall and vault mosaics. Because it is extremely difficult to visually distinguish natural obsidian from man-made glass imitations we present in this paper data collected by means of non-destructive chemico-physical analyses SEM-EDX, portable X-ray fluorescence (p-XRF) and Raman spectroscopy to easily distinguish man-made glass from natural obsidian. In particular the use of portable instruments makes possible in situ analysis of objects in archaeological depots or museum collections to help defining distribution networks to better understand the shifting consumption patterns in Antiquity.
Keywords: A1 Journal article; AXES (Antwerp X-ray Analysis, Electrochemistry and Speciation)
Impact Factor: 0.883
Times cited: 2
DOI: 10.2451/2015PM0026
|