“High-Throughput Morphological Chirality Quantification of Twisted and Wrinkled Gold Nanorods”. Vlasov E, Heyvaert W, Ni B, Van Gordon K, Girod R, Verbeeck J, Liz-Marzán LM, Bals S, ACS Nano (2024). http://doi.org/10.1021/acsnano.4c02757
Abstract: Chirality in gold nanostructures offers an exciting opportunity to tune their differential optical response to left- and right-handed circularly polarized light, as well as their interactions with biomolecules and living matter. However, tuning and understanding such interactions demands quantification of the structural features that are responsible for the chiral behavior. Electron tomography (ET) enables structural characterization at the single-particle level and has been used to quantify the helicity of complex chiral nanorods. However, the technique is time-consuming and consequently lacks statistical value. To address this issue, we introduce herein a high-throughput methodology that combines images acquired by secondary electron-based electron beam-induced current (SEEBIC) with quantitative image analysis. As a result, the geometric chirality of hundreds of nanoparticles can be quantified in less than 1 h. When combining the drastic gain in data collection efficiency of SEEBIC with a limited number of ET data sets, a better understanding of how the chiral structure of individual chiral nanoparticles translates into the ensemble chiroptical response can be reached.
Keywords: A1 Journal Article; Electron Microscopy for Materials Science (EMAT) ;
Impact Factor: 17.1
DOI: 10.1021/acsnano.4c02757
|
“Single Crystal and Pentatwinned Gold Nanorods Result in Chiral Nanocrystals with Reverse Handedness”. Van Gordon K, Ni B, Girod R, Mychinko M, Bevilacqua F, Bals S, Liz‐Marzán LM, Angewandte Chemie International Edition (2024). http://doi.org/10.1002/anie.202403116
Abstract: Handedness is an essential attribute of chiral nanocrystals, having a major influence on their properties. During chemical growth, the handedness of nanocrystals is usually tuned by selecting the corresponding enantiomer of chiral molecules involved in asymmetric growth, often known as chiral inducers. We report that, even using the same chiral inducer enantiomer, the handedness of chiral gold nanocrystals can be reversed by using Au nanorod seeds with either single crystalline or pentatwinned structure. This effect holds for chiral growth induced both by amino acids and by chiral micelles. Although it was challenging to discern the morphological handedness for<italic>L</italic>‐cystine‐directed particles, even using electron tomography, both cases showed circular dichroism bands of opposite sign, with nearly mirrored chiroptical signatures for chiral micelle‐directed growth, along with quasi‐helical wrinkles of inverted handedness. These results expand the chiral growth toolbox with an effect that might be exploited to yield a host of interesting morphologies with tunable optical properties.
Keywords: A1 Journal Article; Electron Microscopy for Materials Science (EMAT) ;
Impact Factor: 16.6
DOI: 10.1002/anie.202403116
|
“Tuning the Growth of Chiral Gold Nanoparticles Through Rational Design of a Chiral Molecular Inducer”. Van Gordon K, Baúlde S, Mychinko M, Heyvaert W, Obelleiro-Liz M, Criado A, Bals S, Liz-Marzán LM, Mosquera J, Nano Letters (2023). http://doi.org/10.1021/acs.nanolett.3c02800
Abstract: The bottom-up production of chiral gold nanomaterials holds great potential for the advancement of biosensing and nano-optics, among other applications. Reproducible preparations of colloidal nanomaterials with chiral morphology have been reported, using cosurfactants or chiral inducers such as thiolated amino acids. However, the underlying growth mechanisms for these nanomaterials remain insufficiently understood. We introduce herein a purposely devised chiral inducer, a cysteine modified with a hydrophobic chain, as a versatile chiral inducer. The amphiphilic and chiral features of this molecule provide control over the chiral morphology and the chiroptical signature of the obtained nanoparticles by simply varying the concentration of chiral inducer. These results are supported by circular dichroism and electromagnetic modeling as well as electron tomography to analyze structural evolution at the facet scale. Our observations suggest complex roles for the factors involved in chiral synthesis: the chemical nature of the chiral inducers and the influence of cosurfactants.
Keywords: A1 Journal Article; Electron Microscopy for Materials Science (EMAT) ;
Impact Factor: 10.8
DOI: 10.1021/acs.nanolett.3c02800
|
“Spontaneous Chirality Evolved at the Au–Ag Interface in Plasmonic Nanorods”. Sa J, Hu N, Heyvaert W, Van Gordon K, Li H, Wang L, Bals S, Liz-Marzán LM, Ni W, Chemistry of materials (2023). http://doi.org/10.1021/acs.chemmater.3c01044
Abstract: Chiral ligands are considered a required ingredient during the synthesis of dissymmetric plasmonic metal nanocrystals. The mechanism behind the generation of chiral structures involves the formation of high Miller index chiral facets, induced by the adsorption of such chiral ligands. We found however that, chirality can also evolve spontaneously, without the involvement of any chiral ligands, during the co-deposition of Au and Ag on Au nanorods. When using a specific Au/Ag ratio, phase segregation of the two metals leads to an interface within the obtained AuAg shell, which can be exposed by removing the Ag component via oxidative etching. Although a close-to-racemic mixture of chiral Au nanorods with right and left handedness is found in solution, electron tomography analysis evidences left- and righthanded helicities, both at the Au-Ag interface and at the exposed surface of Au NRs after Ag etching. The helicity profile of the NRs indicates dominating inclination angles in a range from 30° to 60°. Single-particle optical characterization also reveals random handedness in the plasmonic response of individual nanorods. We hypothesize that, the origin of chirality is related with symmetry breaking during the co-deposition of Au and Ag, through an initial perturbation in a small region on the Au-Ag interface that eventually leads to chiral segregation throughout the nanocrystal.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)