“Toward deep blue nano hope diamonds : heavily boron-doped diamond nanoparticles”. Heyer S, Janssen W, Turner S, Lu Y-G, Yeap WS, Verbeeck J, Haenen K, Krueger A, ACS nano 8, 5757 (2014). http://doi.org/10.1021/nn500573x
Abstract: The production of boron-doped diamond nanoparticles enables the application of this material for a broad range of fields, such as electrochemistry, thermal management, and fundamental superconductivity research. Here we present the production of highly boron-doped diamond nanoparticles using boron-doped CVD diamond films as a starting material. In a multistep milling process followed by purification and surface oxidation we obtained diamond nanoparticles of 1060 nm with a boron content of approximately 2.3 × 1021 cm3. Aberration-corrected HRTEM reveals the presence of defects within individual diamond grains, as well as a very thin nondiamond carbon layer at the particle surface. The boron K-edge electron energy-loss near-edge fine structure demonstrates that the B atoms are tetrahedrally embedded into the diamond lattice. The boron-doped diamond nanoparticles have been used to nucleate growth of a boron-doped diamond film by CVD that does not contain an insulating seeding layer.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 13.942
Times cited: 71
DOI: 10.1021/nn500573x
|
|
|
“Substitutional phosphorus incorporation in nanocrystalline CVD diamond thin films”. Janssen W, Turner S, Sakr G, Jomard F, Barjon J, Degutis G, Lu YG, D'Haen J, Hardy A, Bael MV, Verbeeck J, Van Tendeloo G, Haenen K, Physica status solidi: rapid research letters 8, 705 (2014). http://doi.org/10.1002/pssr.201409235
Abstract: Nanocrystalline diamond (NCD) thin films were produced by chemical vapor deposition (CVD) and doped by the addition of phosphine to the gas mixture. The characterization of the films focused on probing the incorporation and distribution of the phosphorus (P) dopants. Electron microscopy evaluated the overall film morphology and revealed the interior structure of the nanosized grains. The homogeneous films with distinct diamond grains featured a notably low sp(2):sp(3)-ratio as confirmed by Raman spectroscopy. High resolution spectroscopy methods demonstrated a homogeneous P-incorporation, both in-depth and in-plane. The P concentration in the films was determined to be in the order of 10(19) cm(-3) with a significant fraction integrated at substitutional donor sites. (C) 2014 WILEY-VCH Verlag GmbH Co. KGaA, Weinheim
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 3.032
Times cited: 20
DOI: 10.1002/pssr.201409235
|
|