“Combination of CeO2 and PtO2 doping for the strong enhancement of Jc under magnetic field in melt-textured superconductor YBaCuO”. Delamare MP, Hervieu M, Wang J, Provost J, Monot I, Verbist K, Van Tendeloo G, Physica: C : superconductivity 262, 220 (1996). http://doi.org/10.1016/0921-4534(96)00225-0
Abstract: A combination of CeO2 and PtO2 doping has been studied in melt-processed YBa2Cu3O7-x. This study was carried out using an optimized well established MTG process. The cerium-platinum doped samples exhibit a high fishtail effect with a J(c) of 4.3 x 10(4) A/cm(2) under an applied field of 1 T. Microstructural and nanostructural studies have been performed. The 211 and BaCeO3 inclusions are a few micrometers wide and the formation of a metastable nanocrystalline phase (Y4Ba4)Cu-8-x(Ce,Pt)(x)O-20+delta related to the perovskite is detected. The 123 grains show no specific extended defect generated by the doping process. The relationship between structure and properties are discussed.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 0.942
Times cited: 27
DOI: 10.1016/0921-4534(96)00225-0
|
|
|
“Microstructure and flux pinning properties of melt textured grown doped YBa2Cu3O7-\delta”. Monot I, Verbist K, Hervieu M, Laffez P, Delamare MP, Wang J, Desgardin G, Van Tendeloo G, Physica: C : superconductivity 274, 253 (1997)
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 1.404
Times cited: 33
|
|
|
“Interfacial dielectric layer as an origin of polarization fatigue in ferroelectric capacitors”. Do MT, Gauquelin N, Nguyen MD, Wang J, Verbeeck J, Blom F, Koster G, Houwman EP, Rijnders G, Scientific Reports 10, 7310 (2020). http://doi.org/10.1038/s41598-020-64451-0
Abstract: Origins of polarization fatigue in ferroelectric capacitors under electric field cycling still remain unclear. Here, we experimentally identify origins of polarization fatigue in ferroelectric PbZr0.52Ti0.48O3 (PZT) thin-film capacitors by investigating their fatigue behaviours and interface structures. The PZT layers are epitaxially grown on SrRuO3-buffered SrTiO3 substrates by a pulsed laser deposition (PLD), and the capacitor top-electrodes are various, including SrRuO3 (SRO) made by in-situ PLD, Pt by in-situ PLD (Pt-inPLD) and ex-situ sputtering (Pt-sputtered). We found that fatigue behaviour of the capacitor is directly related to the top-electrode/PZT interface structure. The Pt-sputtered/PZT/SRO capacitor has a thin defective layer at the top interface and shows early fatigue while the Pt-inPLD/PZT/SRO and SRO/PZT/SRO capacitor have clean top-interfaces and show much more fatigue resistance. The defective dielectric layer at the Pt-sputtered/PZT interface mainly contains carbon contaminants, which form during the capacitor ex-situ fabrication. Removal of this dielectric layer significantly delays the fatigue onset. Our results clearly indicate that dielectric layer at ferroelectric capacitor interfaces is the main origin of polarization fatigue, as previously proposed in the charge injection model.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 4.6
Times cited: 18
DOI: 10.1038/s41598-020-64451-0
|
|
|
“Triple-Modal Imaging of Magnetically-Targeted Nanocapsules in Solid TumoursIn Vivo”. Bai J, Wang JT-W, Rubio N, Protti A, Heidari H, Elgogary R, Southern P, Al-Jamal W' T, Sosabowski J, Shah AM, Bals S, Pankhurst QA, Al-Jamal KT, Theranostics 6, 342 (2016). http://doi.org/10.7150/thno.11918
Abstract: Triple-modal imaging magnetic nanocapsules, encapsulating hydrophobic superparamagnetic iron oxide nanoparticles, are formulated and used to magnetically target solid tumours after intravenous administration in tumour-bearing mice. The engineered magnetic polymeric nanocapsules m-NCs are ~200 nm in size with negative Zeta potential and shown to be spherical in shape. The loading efficiency of superparamagnetic iron oxide nanoparticles in the m-NC was ~100%. Up to ~3- and ~2.2-fold increase in tumour uptake at 1 and 24 h was achieved, when a static magnetic field was applied to the tumour for 1 hour. m-NCs, with multiple imaging probes (e.g. indocyanine green, superparamagnetic iron oxide nanoparticles and indium-111), were capable of triple-modal imaging (fluorescence/magnetic resonance/nuclear imaging) in vivo. Using triple-modal imaging is to overcome the intrinsic limitations of single modality imaging and provides complementary information on the spatial distribution of the nanocarrier within the tumour. The significant findings of this study could open up new research perspectives in using novel magnetically-responsive nanomaterials in magnetic-drug targeting combined with multi-modal imaging.
Keywords: A1 Journal article; Electron microscopy for materials research (EMAT)
Impact Factor: 8.712
Times cited: 54
DOI: 10.7150/thno.11918
|
|