“Damage mechanisms in selective laser melted AlSi10Mg under as built and different post-treatment conditions”. Zhao L, Macias JGS, Ding L, Idrissi H, Simar A, Microstructure And Processing 764, 138210 (2019). http://doi.org/10.1016/J.MSEA.2019.138210
Abstract: Selective laser melting (SLM) manufactured AlSi10Mg alloys present a fine silicon-rich network and precipitates which grant high mechanical strength but low ductility. Post-treatments, aiming at eliminating inherent defects related to SLM such as residual stresses, porosity or inhomogeneity, result in significant changes in the microstructure and impact both the hardening and the damage mechanisms of the post-treated material. The present work is dedicated to the investigation of the fracture of SLM AlSi10Mg under as built and three post-treatment conditions, namely two stress relieve heat treatments and friction stir processing (FSP). It is found that the interconnected Si network fosters damage at low strain due to the brittleness of the Si phase. The onset of damage transfers load to the enclosed Al phase which then fractures quickly under high stress, thus leading to low material ductility. In contrast, when the Si network is globularized into Si particles, the ductility is highly increased even in the case where the porosity and inhomogeneity of the microstructure remain after the post-treatment. The ductility enhancement results from the delay in void nucleation on the Si particles as well as from the tolerance for void growth in the Al matrix.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 3.094
Times cited: 1
DOI: 10.1016/J.MSEA.2019.138210
|
|
|
“Clustering behavior during natural aging and artificial aging in Al-Mg-Si alloys with different Ag and Cu addition”. Weng Y, Jia Z, Ding L, Muraishi S, Liu Q, Microstructure And Processing 732, 273 (2018). http://doi.org/10.1016/J.MSEA.2018.07.018
Abstract: The effect of Ag and Cu addition on clustering behavior of Al-Mg-Si alloys during natural aging (NA) and artificial aging (AA) was investigated by hardness measurement, tensile test and atom probe tomography analysis. The results show that both Ag and Cu atoms could enter clusters and GP-zones, change the Mg/Si ratio and increase their volume fractions. Compared with the Al base alloy, the clusters in the Ag/Cu-added alloys more easily transform to beta" phases for size and compositional similarity, and the strengthening ability of these particles is enhanced by the increased volume fraction and shear modulus. In NA condition, Cu is greater in improving the volume fraction of clusters than Ag and thus produces higher T4 temper hardness. In AA condition, in contrary, Ag is more effective in facilitating the formation and growth of particles than Cu due to the stronger Ag-Mg interaction and the high diffusivity of Ag atoms in Al matrix, leading to highest hardening response. Compared to the Cu-added alloy, the Ag-added alloy shows higher precipitation kinetics during AA treatment and maintains a lower T4 temper hardness.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 3.094
Times cited: 11
DOI: 10.1016/J.MSEA.2018.07.018
|
|
|
“Au particles supported on (110) anatase-TiO2”. Giorgio S, Henry CR, Pauwels B, Van Tendeloo G, Microstructure And Processing 297, 197 (2001). http://doi.org/10.1016/S0921-5093(00)01261-2
Abstract: Au particles were prepared by evaporation in ultra high vacuum at high temperature, on the surfaces of TiO2 micro-spheres with the anatase structure. The morphology and the structural deformation in Au deposits were studied by high resolution transmission electron microscopy and image simulations by the multislice technique. The particles were polyhedral, limited by (100) and (111) faces. Patches with a hexagonal lattice were found around the particles, which was interpreted as thin Au islands on the surface. In these islands the Au lattice was deformed and perfectly accommodated to the (110) surface of TiO2. (C) 2001 Elsevier Science B.V. All rights reserved.
Keywords: A1 Journal article; Engineering sciences. Technology; Electron microscopy for materials research (EMAT)
Impact Factor: 3.094
Times cited: 40
DOI: 10.1016/S0921-5093(00)01261-2
|
|